Precious Metal Recovery in Zimbabwe
The final stage of gold recovery: turning strip solutions into physical metal you can hold in your hand. We recover gold, silver, and other precious metals through electrowinning and smelting, with full chain-of-custody documentation.
From Strip Solution to Physical Gold
After gold elution strips the precious metals from your loaded carbon, the gold sits dissolved in a strip solution. This solution, often called pregnant solution or pregnant eluate, contains gold, silver, and sometimes trace amounts of other metals.
The next step is electrowinning. The pregnant solution flows through a series of electrowinning cells where a direct electrical current is applied. Gold and silver ions in the solution are attracted to steel wool cathodes, where they deposit as a dark sludge. The barren solution, now mostly free of gold, is recycled back into the elution circuit.
Electrowinning is remarkably efficient when done properly. With correct cell design, voltage settings, and solution flow rates, we typically recover 99% or more of the gold from the strip solution. The key is maintaining clean cells, proper cathode contact, and consistent solution chemistry.
Once the cathodes are loaded with enough gold sludge, they are removed from the cells. The sludge is washed, dried, and weighed. It is then mixed with fluxes, specific chemical additives that help separate the precious metals from impurities, and smelted in a furnace.
The result is a dore bar: a rough alloy bar that is typically 70% to 90% gold, with the balance being silver and minor impurities. This bar is weighed, assayed, and documented before being sent to a licensed refinery such as Fidelity Gold Refinery for final purification.
Chain of Custody and Security
Arrival Documentation
Every batch of carbon is weighed, photographed, and sampled on arrival. You receive a receipt with weights and batch reference numbers.
Process Tracking
Strip solutions are sampled at multiple points during elution and electrowinning. All samples are assayed and recorded.
Final Reconciliation
Your report includes input weights, assay results, gold and silver recovered, and a mass balance that accounts for every gram in the system.
Materials We Accept
We process loaded activated carbon from any gold recovery operation. This includes carbon from CIP plants, CIL plants, heap leach operations, and smaller artisanal setups. The carbon must have adsorbed gold or silver that needs recovery.
We also handle existing pregnant solutions from other facilities, cathode sludge for smelting, and gravity concentrates that need further refining. If you have gold-bearing material and need it converted to a dore bar or pure metal, talk to us about what you have.
Materials that contain mercury, arsenic, or other hazardous contaminants may require special handling or pre-treatment. Let us know what you are working with before delivery so we can prepare accordingly.
Expected Recovery Rates
Overall recovery, from loaded carbon through elution and electrowinning to final dore bar, typically ranges from 95% to 99%. The exact figure depends on several factors:
- Carbon condition and gold loading level
- Strip solution chemistry and concentration
- Number of elution cycles the carbon has been through
- Presence of contaminants or carbon fouling
- Electrowinning cell efficiency and maintenance
We monitor every variable that affects recovery. If we see something that could reduce your yield, such as carbon fouling or unusual solution chemistry, we will flag it and discuss options before proceeding.
Recovery FAQ
Ready to Recover Your Precious Metals?
Tell us about your material and we will outline the recovery process and expected results.