Top 5 Problems That Reduce Gold Elution Efficiency (and How to Fix Them)

Top 5 Problems That Reduce Gold Elution Efficiency (and How to Fix Them)

Bulawayo ElutionsNov 15, 2026 7 min read

When Elution Performance Dips, Gold Stays on Carbon

Gold elution is the final stretch, the part of the process where months of hard work in the pit finally translate into physical metal. But when elution performance dips, even slightly, the losses can be serious. A drop from 98% stripping efficiency to 92% might not sound dramatic, but on a batch of carbon loaded at 5,000 g/t, that is 300 grams of gold per tonne of carbon left behind. At current gold prices, those grams add up fast.

The good news is that most elution efficiency problems have identifiable causes and practical fixes. Here are the five most common ones we see at our facility in Bulawayo.

Problem 1: Carbon Fouling

Carbon fouling is the number one cause of poor elution performance. When the pores and surface of activated carbon get blocked by deposits, gold cannot desorb efficiently. The strip solution cannot reach the gold that is trapped deep in fouled pores, and the gold that is on the surface has trouble releasing because contaminants interfere with the chemical equilibrium.

Common foulants include:

  • Calcium carbonate (CaCO3) from hard water in the leach circuit
  • Organic compounds from flotation reagents, oils, and naturally occurring organics in the ore
  • Fine silica and clay particles that coat the carbon surface
  • Iron and manganese oxides from groundwater or acidic leach conditions

How to fix it:

  • Acid wash the carbon with 3% to 5% HCl before elution to remove inorganic deposits. This is built into the AARL process and should be done as a pre-treatment for ZADRA runs when fouling is evident.
  • Thermally regenerate carbon in a kiln at 650 to 750 degrees C to burn off organic foulants. This should be done every 3 to 5 elution cycles.
  • Address the source: treat your process water, manage flotation reagent carry-over, and screen out fines from the carbon circuit.

Read our detailed guide on carbon processing for more on carbon maintenance.

Problem 2: Strip Solution Chemistry

The strip solution does the actual work of pulling gold off carbon. If its chemistry is wrong, stripping slows down or stalls altogether.

Common issues:

  • Caustic (NaOH) concentration too low: the pH is not high enough to displace gold from the carbon
  • Cyanide (NaCN) concentration too high: excess cyanide can actually inhibit desorption at certain concentrations
  • Solution contaminated with calcium or other ions from poor-quality water
  • Solution not being refreshed often enough, leading to buildup of dissolved impurities

How to fix it:

  • Test your strip solution chemistry before each cycle. Target 1% to 2% NaOH and 0.1% to 0.5% NaCN for most applications.
  • Use deionised or demineralised water for AARL systems. Softened water at minimum for ZADRA.
  • Replace or refresh strip solution regularly. Do not keep recycling the same batch indefinitely.
  • Monitor solution pH and free cyanide levels throughout the cycle.

Problem 3: Temperature Control

Temperature is the main driving force in gold elution. At higher temperatures, the equilibrium shifts strongly in favour of desorption. If your temperature drops or fluctuates during the cycle, stripping slows down.

Common issues:

  • Boiler or heat exchanger not maintaining target temperature
  • Heat loss through uninsulated piping and columns
  • Fluctuating temperatures during the cycle due to variable fuel supply or electrical issues
  • Temperature measured at the wrong point (inlet vs column midpoint vs outlet)

How to fix it:

  • Insulate all piping, columns, and heat exchangers. Heat loss is free money walking out the door.
  • Calibrate temperature sensors and place them at meaningful points (column inlet and outlet at minimum).
  • Maintain boilers and heat exchangers on a regular schedule. A boiler running at 80% efficiency wastes fuel and may not reach target temperatures.
  • For AARL, ensure your pressure system is holding at the correct pressure to maintain the required temperature above 100 degrees C.

Problem 4: Flow Distribution Problems

Even if your solution chemistry and temperature are perfect, poor flow distribution through the carbon bed will leave gold behind. If the solution channels through one part of the bed and bypasses another, the bypassed carbon barely gets stripped.

Common issues:

  • Carbon bed not evenly packed in the column
  • Fine carbon particles blocking flow in certain areas
  • Column screens damaged or blocked, creating uneven flow
  • Air pockets in the column preventing solution contact with all the carbon

How to fix it:

  • Screen out fine carbon particles before loading the column. Fines below 1mm cause the most flow problems.
  • Load the column carefully, ensuring even distribution. Do not dump all the carbon in from one side.
  • Check and maintain column screens regularly. Replace damaged screens immediately.
  • Bleed air from the system before starting the circulation. Air pockets are especially problematic in pressurised AARL systems.
  • Monitor pressure differential across the column. A sudden increase indicates blockage.

Problem 5: Water Quality

Water quality is often overlooked because it seems like a minor input. But the water you use to make up your strip solution directly affects every chemical reaction in the elution process.

Common issues:

  • High total dissolved solids (TDS) in the water, especially calcium and magnesium
  • Water pH outside the optimal range
  • Chlorides in the water corroding equipment and interfering with cyanide chemistry
  • Organic matter in the water adding to carbon fouling

How to fix it:

  • Test your water source regularly for TDS, hardness, pH, chlorides, and organics.
  • Use deionised water for AARL elution. Softened water for ZADRA at minimum.
  • Install appropriate water treatment: reverse osmosis, ion exchange, or simple softening depending on your water quality issues.
  • Do not use borehole water directly without treatment if TDS is above 200 mg/L.

We have written a comprehensive guide on how water quality affects gold elution efficiency that covers this topic in detail.

Putting It All Together

These five problems rarely occur in isolation. Carbon fouling leads to longer cycle times, which puts more stress on solution chemistry and temperature control. Poor water quality causes carbon fouling and solution contamination simultaneously. Flow distribution problems get worse as fines accumulate from degraded carbon.

The best approach is systematic: address all five areas as part of a regular maintenance and quality control program. Check carbon condition before every elution run. Test strip solution chemistry. Verify temperatures and flow rates. Test your water. Keep records so you can spot trends before they become problems.

At Bulawayo Elutions, we monitor all of these variables on every batch. If we see something that could affect your recovery, we flag it and discuss options before proceeding. Get in touch if you are experiencing elution efficiency issues.

Frequently Asked Questions

What is a good stripping efficiency target?

For AARL systems, aim for 97% or higher. For ZADRA, 93% to 96% is typical for a well-managed system. Anything below 90% indicates a significant problem that needs investigation.

How do I know if my carbon is fouled?

Signs include declining gold recovery in the adsorption circuit, longer elution times, lower stripping efficiency compared to previous batches of the same carbon, and a visual change from shiny black to dull or coated appearance.

Can poor elution efficiency be fixed without replacing the carbon?

Often, yes. Acid washing removes inorganic foulants, thermal regeneration burns off organics, and fixing solution chemistry and temperature issues can restore performance. Carbon only needs replacing when it has lost too much physical structure or activity after regeneration.